Halogen-free Flame Retardant Reinforced PC HF-1012G10

Halogen-free Flame Retardant Reinforced PC HF-1012G10. Tensile strength 80 MPa, Notched impact 120 J/m. MOQ 500 kg.

HF-1012G10PC Modified PolycarbonateQingdao plant
Halogen-free Flame Retardant Reinforced PC HF-1012G10
Grade
HF-1012G10
Family
ABS Modified Series
Form
Pellets, 25 kg bags
MOQ
500 kg
Color
Natural · matched to your color standard
Customisation
Color and properties adjusted to your requirements
Download TDS (PDF)Chinese version

Typical Properties (TDS)

Values are typical and measured under standard ISO methods; refer to the lot COA for release data.
PropertyUnitTypical value
Density (23℃)g/cm³1.26
Mould shrinkage (23℃)%0.3-0.5
MFR (300℃/1.2kg)g/10min13
Tensile strength (50mm/min)MPa80
Elongation at break (50mm/min)%10
Flexural strength (2.0mm/min)MPa125
Flexural modulus (2.0mm/min)MPa4020
Notched impact strength (23℃)J/m120
HDT (1.82MPa)°C142
Flammability (1.5mm)—V0
Typical value ranges are for grade screening and preliminary comparison. Purchases are governed by the agreed technical specification or sealed reference sample, with a COA shipped on every lot.

Recommended Processing

ParameterRecommended
Drying120℃, 4.0h
Rear zone temperature265℃-280℃
Middle zone temperature270℃-290℃
Front zone temperature270℃-290℃
Nozzle temperature270℃-290℃
Melt temperature275℃-295℃
Mould temperature110℃-115℃

Typical Applications

  • Precision electronics housings
  • Explosion-protected parts
  • Instrument cases

Other Grades in This Family

Need the full data sheet and a quote for HF-1012G10?

Tell us the wall thickness, service temperature and volume, and we will come back within 24 hours with a technical recommendation and pricing.

FAQ

Can Halogen-free Flame Retardant Reinforced PC HF-1012G10 replace the grade we are using now?

Yes. Send us the incumbent grade and the critical values (tensile strength, impact at −30 °C, shrinkage, colour) and we match the formulation to those targets. Most customers validate with a 5–25 kg sample before switching production.

Why can two compounds with the same grade name differ by 15% in strength?

Fibre length retention and the coupling system. We control shear on twin-screw lines and test every lot for MFR, ash, tensile and impact; each lot ships with a COA for traceability.

What are the typical properties of Halogen-free Flame Retardant Reinforced PC HF-1012G10?
Typical properties of Halogen-free Flame Retardant Reinforced PC HF-1012G10 (ISO test methods; indicative values — certified results in the batch COA):Density 1.26 g/cm³; Mould shrinkage 0.3-0.5 %; MFR 13 g/10min; Tensile strength 80 MPa; Elongation at break 10 %; Flexural strength 125 MPa; Flexural modulus 4020 MPa; Notched impact strength 120 J/m; HDT 142 °C; Flammability V0
What injection moulding conditions are recommended for Halogen-free Flame Retardant Reinforced PC HF-1012G10?
Recommended processing conditions for Halogen-free Flame Retardant Reinforced PC HF-1012G10:Drying 120℃, 4.0h; Rear zone temperature 265℃-280℃; Middle zone temperature 270℃-290℃; Front zone temperature 270℃-290℃; Nozzle temperature 270℃-290℃; Melt temperature 275℃-295℃; Mould temperature 110℃-115℃
What is Halogen-free Flame Retardant Reinforced PC HF-1012G10 typically used for?
Halogen-free Flame Retardant Reinforced PC HF-1012G10 is typically used in:Precision electronics housings, Explosion-protected parts, Instrument cases
What is the minimum order quantity for Halogen-free Flame Retardant Reinforced PC HF-1012G10?
Minimum order quantity is 500 kg for standard grades and 1 tonne for newly developed custom formulations.
Can Halogen-free Flame Retardant Reinforced PC HF-1012G10 be tailored to specific performance targets?
Yes. Qingdao Yunsu adjusts formulations to the target requirements, including glass fibre loading, flame-retardant class, UV and weathering resistance, antistatic or conductive properties and colour, and supports dedicated grade development.
How long do sampling and mass production take?
Sampling takes 3-7 days for existing grades and 7-15 days for new formulations; mass production runs 10-20 days after sample approval, shipping from Qingdao Port.
Can the color and properties be customized to our requirements?
Yes. Colours can be matched to your colour standard. Give us the working conditions, performance targets and cost ceiling — we design the formulation backwards from there. Most customers validate with a 5–25 kg sample before series production.
Call Email