Reinforced Toughened PA6 RF-1332GF25
Tensile strength 125 MPa, Notched impact strength 290 J/m.
Request Data Sheet & Quote →Modified PA6 TM-1332T10. Tensile strength 40 MPa, Notched impact 20 kJ/m². MOQ 500 kg.

| Property | Unit | Typical value |
|---|---|---|
| Density (23℃) | g/cm³ | 1.12 |
| Mould shrinkage (23℃) | % | 1.1-1.5 |
| MFR (250℃ 2.16kg) | g/10min | 10 |
| Tensile strength (50mm/min) | MPa | 40 |
| Elongation at break (50mm/min) | % | 155 |
| Flexural strength (2mm/min) | MPa | 50 |
| Flexural modulus (2mm/min) | MPa | 1450 |
| Notched impact strength (23℃) | kJ/m² | 20 |
| HDT (1.8MPa) | °C | 62 |
| Flammability | — | HB |
| Parameter | Recommended |
|---|---|
| Drying | 100℃, 4.0h |
| Rear zone temperature | 230℃ |
| Middle zone temperature | 220℃-240℃ |
| Front zone temperature | 230℃-250℃ |
| Nozzle temperature | 240℃-250℃ |
| Melt temperature | 230℃-250℃ |
| Mould temperature | 60℃-100℃ |

Tensile strength 125 MPa, Notched impact strength 290 J/m.
Request Data Sheet & Quote →
Tensile strength 120 MPa, Notched impact strength 29 kJ/m².
Request Data Sheet & Quote →
Tensile strength 52 MPa, Notched impact strength 60 J/m.
Request Data Sheet & Quote →
Tensile strength 110 MPa, Notched impact strength 10.5 kJ/m².
Request Data Sheet & Quote →Tell us the wall thickness, service temperature and volume, and we will come back within 24 hours with a technical recommendation and pricing.
Yes. Send us the incumbent grade and the critical values (tensile strength, impact at −30 °C, shrinkage, colour) and we match the formulation to those targets. Most customers validate with a 5–25 kg sample before switching production.
Fibre length retention and the coupling system. We control shear on twin-screw lines and test every lot for MFR, ash, tensile and impact; each lot ships with a COA for traceability.